Why Lubricate Nylon?

Nylon’s natural surface properties include a relatively low coefficient of friction compared to many engineering plastics—but it’s not inherently self-lubricating. In moving-part applications like gears, bearings, slides, and cams, unlubricated nylon can experience accelerated wear, frictional heating, and stick-slip behavior. Lubricated nylon grades solve this by incorporating solid or liquid lubricants directly into the polymer matrix, creating parts that run smoothly for millions of cycles without external lubrication.

The lubricant additives work by forming a transfer film on the mating surface. As the nylon part moves, microscopic lubricant particles are released, coating both the nylon surface and the opposing metal or plastic surface. This film reduces the coefficient of friction from 0.35–0.40 (unmodified nylon on steel) down to 0.10–0.20, depending on the lubricant type and loading.

The Three Main Lubricant Types

Lubricant Typical Loading COF (vs Steel) Лучшее приложение
PTFE (тефлон) 10–20% 0.10–0.18 High-speed bearings, low-load slides
MoS₂ (Molybdenum Disulfide) 1–5% 0.12–0.20 High-load gears, thrust washers
Oil-filled 2–8% 0.08–0.15 Precision bearings, low-noise applications

PTFE-Filled Nylon

PTFE (polytetrafluoroethylene) is the most common solid lubricant for nylon. With a coefficient of friction as low as 0.04 in its pure form, PTFE particles dispersed throughout nylon create an extremely low-friction surface. PTFE-filled nylons are ideal for high-speed, low-to-moderate load applications where continuous sliding motion is required.

The limitation: PTFE reduces mechanical strength by 10–20% and increases cost. It also doesn’t perform as well as MoS₂ under very high contact pressures.

MoS₂-Filled Nylon

Molybdenum disulfide has a layered crystal structure similar to graphite—sheets that easily slide past each other. This makes it exceptional under high contact pressures where PTFE would be squeezed out. MoS₂-filled nylon is the go-to choice for gears, cams, and thrust washers operating under significant load.

MoS₂ also increases nylon’s crystallinity slightly, which can improve strength and stiffness—unlike PTFE which weakens the matrix. The dark gray/black color can be a consideration for visible parts.

Oil-Filled Nylon

Oil-filled nylons incorporate lubricating oil directly into the polymer during compounding. During operation, the oil slowly migrates to the surface, providing continuous lubrication throughout the part’s life. This “self-replenishing” characteristic makes oil-filled nylon excellent for sealed applications where relubrication is impossible.

Common oils include silicone, mineral oil, and synthetic hydrocarbon oils. The oil content is precisely controlled to avoid excessive migration that could contaminate surrounding components.

Content image
Иллюстрация к тексту

Wear Rate Comparison

Марка нейлона K-Factor (×10⁻⁸ mm³/N·m) PV Limit (MPa·m/s) Service Temp Range
PA6 без наполнителя 40–80 0.09–0.12 -30°C to 85°C
PA6 + 15% PTFE 5–12 0.15–0.25 -40°C to 100°C
PA6 + MoS₂ 8–15 0.20–0.35 -30°C to 95°C
PA66 + Aramid + PTFE 2–5 0.35–0.50 -40°C to 120°C

Design Guidelines for Lubricated Nylon Parts

  • Surface finish of the mating part: Aim for 0.2–0.4 μm Ra on the steel/opposing surface. Rougher surfaces accelerate wear.
  • Clearance: Allow 0.3–0.5% of the bearing diameter for thermal expansion and water absorption swell.
  • Толщина стенки: Maintain uniform wall thickness to avoid warpage that creates uneven wear patterns.
  • Running-in period: Expect higher friction during the first 500–1000 cycles as the transfer film establishes.
  • Combination with glass fiber: Adding glass fiber to lubricated nylon improves load capacity but increases wear on the mating surface. Use hardened steel (58+ HRC) for mating parts.

Почему стоит выбрать нейлоновый пластик для своих инженерных нужд?

  • ✅ 300+ термопластавтоматов от 50T до 2000T
  • ✅ 10 000+ деталей в день производственные мощности
  • ✅ Точность ±0,02 мм допуск на все материалы
  • ✅ MOQ только 1 шт. для создания прототипов; масштабируется до миллионов
  • ✅ Круглосуточное цитирование, Срок изготовления 3-15 дней
  • ✅ Сертифицированная система менеджмента качества ISO 9001

Получите предложение в течение 24 часов →

Похожие статьи

ЧАСТО ЗАДАВАЕМЫЕ ВОПРОСЫ

How do you know whether Lubricated Nylon Grades: PTFE, MoS₂ and Oil-Filled Options for Wear Applications fits a part?

Lubricated Nylon Grades: PTFE, MoS₂ and Oil-Filled Options for Wear Applications fits a part when its load capacity, temperature range, moisture exposure, wear behavior, and processing method match the real service conditions.

What properties should be checked for Lubricated Nylon Grades: PTFE, MoS₂ and Oil-Filled Options for Wear Applications?

Проверить прочность, жесткость, ударопрочность, термостойкость, влагопоглощение, стабильность размеров, коэффициент трения, износостойкость и химическую совместимость.

What is the biggest selection risk for Lubricated Nylon Grades: PTFE, MoS₂ and Oil-Filled Options for Wear Applications?

Наибольший риск заключается в том, чтобы ориентироваться на значения из технического паспорта, не учитывая реальные условия эксплуатации, метод обработки, геометрию детали и долгосрочную эксплуатацию.

When should Lubricated Nylon Grades: PTFE, MoS₂ and Oil-Filled Options for Wear Applications be tested before production?

Проведение испытаний рекомендуется в случаях, когда деталь подвергается воздействию нагрузок, высоких температур, химических веществ, влаги, должна соответствовать жестким допускам, нормативным требованиям или эксплуатироваться в новых условиях.

Расскажите нам о вашей детали

Это поле обязательно для заполнения.
Это поле обязательно для заполнения.
Это поле обязательно для заполнения.
Это поле обязательно для заполнения.
Это поле обязательно для заполнения.
Это поле обязательно для заполнения.
Это поле обязательно для заполнения.

Related Reading

Прокрутить к верху