ABS CF20 Carbon Fiber Reinforced Pellets

ABS CF20 is a carbon-fiber-reinforced ABS pellet material, referenced here as ABS WHC20A. It can be evaluated for equipment shells, structural mounting parts and fixtures. Select it using the exact grade data and the checks required for the component.

Reference grade: ABS WHC20A

Supply: 20% carbon fiber reinforced pellets. Confirm color, quantity and required documents with your inquiry.

Категория:

ABS CF20 Material Overview

ABS CF20 is a carbon-fiber-reinforced ABS pellet material, referenced here as ABS WHC20A. It can be evaluated for equipment shells, structural mounting parts and fixtures. Select it using the exact grade data and the checks required for the component.

Артикул Подробности
Reference grade ABS WHC20A
Polymer ABS
Reinforcement 20% carbon fiber
Form Pellets for material-supply inquiries
Color and processing Confirm the offered grade and current processing guidance

Reference Material Properties

Typical values for ABS WHC20A from the linked supplier PDF.

Недвижимость Типичное значение Метод испытания
Прочность на разрыв 82 МПа ISO 527
Прочность на изгиб 86 MPa ISO 178
Модуль упругости при изгибе 7800 MPa ISO 178
Notched impact strength 5.6 kJ/m² ISO 180

Specimen conditioning is not stated in the reference sheet. These values are not guaranteed specification limits. Only rows with a usable property, unit and method are reproduced; request clarification of the remaining sheet entries before relying on them for design.

Download ABS WHC20A supplier reference datasheet (PDF)

Application Review

ABS CF20 illustrative component applications
Illustrative component concepts. Confirm the selected formulation for the actual part.

Equipment shells

Define attachment points, openings and cosmetic surfaces. Evaluate filling, weld lines and fit around the internal assembly.

Reinforced mounting parts

Check the loading at ribs, inserts and bolt holes rather than judging suitability from the fiber percentage.

Precision fixtures

Specify the locating features and dimensional acceptance conditions. Validate creep and repeatability under the intended clamping cycle.

Processing and Part Checks

Use the current WHC20A molding guidance. Agree the allowed color and finish, then check dimensional repeatability, insert areas and impact-sensitive edges during trials. Evaluate electrical behavior separately when it is a functional requirement.

For component production, review our injection molding service. For other resin options, browse engineering plastic materials.

Material Supply and Manufacturing Support

Нейлон Пластик connects engineering plastic supply with custom manufacturing. WANHAN is our cooperating compounding factory; the photographs below show its material-feeding equipment, extrusion process and laboratory.

Material feeding equipment at WANHAN, Nylon Plastic’s cooperating factory
Material feeding
Extruded plastic strands at the WANHAN cooperating factory
Extrusion process
Laboratory work area at the WANHAN cooperating factory
Laboratory

Grade and formulation selection

Share your current grade, application and operating conditions. We coordinate the material review and identify the matching datasheet for the formulation offered.

Quality documents for your order

Specify the TDS, batch records, inspection requirements or compliance files your purchasing team needs. The documents and acceptance criteria are agreed for the quoted material.

Support beyond resin pellets

For a finished component, connect material selection with part design, tooling and molding review. Start with the drawing, expected quantity and critical dimensions.

Cooperating Factory Management-System Certificates

The supplied ISO 9001, ISO 14001 and ISO 45001 certificates identify Guangdong Wanhan as the certified entity. Their scope concerns modified plastic granules and the related management activities; it does not certify every material grade or every finished-part manufacturing service.

Review manufacturing capabilities and quality documentation. For document approval, match the legal entity, certificate scope and quoted grade.

Часто задаваемые вопросы

What material does this page cover?

ABS CF20 is a carbon-fiber-reinforced ABS pellet material, referenced here as ABS WHC20A. It can be evaluated for equipment shells, structural mounting parts and fixtures. Select it using the exact grade data and the checks required for the component.

Is ABS CF20 automatically stiffer than ABS CF10?

No. Compare the exact formulations and test conditions. The two reference PDFs list different mechanical values, and their conditioning is not stated. Fiber percentage on its own is not a performance ranking.

Are these values a production specification?

No. They are typical reference values for ABS WHC20A. Agree the current grade, test conditions, acceptance limits and required documents for the order.

Do the images show the exact supplied color and finished parts?

The images illustrate resin appearance and possible component concepts. Confirm color and finish on the offered material and samples; the pictured parts do not establish suitability for your design.

What is required for a material replacement?

Identify the current resin and reason for changing it. Compare exact-grade data, dimensions, loads, temperature and environmental exposure, then validate the intended part before production.

What should I send for a quote or sample request?

Send the reference grade, application, color, estimated material quantity and required documents. For a molded-part inquiry, add the drawing, critical dimensions and acceptance requirements. A CAD file is optional for a material-only inquiry.

Related Material Grades

ABS CF10   |   ABS CF30

Request Material Data and a Quote

Share the grade, application, service conditions, color, quantity and required documents so the offered material can be reviewed against your project.

Request ABS WHC20A TDS and Quote